Explanation
The blast furnace
Iron oxide ore, coke and limestone are fed in at the top. Hot air is blown in at the bottom.
Coke burns at the bottom, reaching about 2170 kelvin, and makes carbon monoxide.
Reduction in the cooler zone
In the upper, cooler zone, carbon monoxide reduces iron oxide step by step.
Fe₂O₃ goes to Fe₃O₄, then to FeO, then to iron.
Limestone makes slag
Limestone breaks down into lime, CaO.
Lime combines with the silica gangue to form calcium silicate slag, which floats on the molten iron and protects it.
Kinds of iron
Pig iron from the blast furnace has about 4 percent carbon.
Cast iron, made by remelting it with scrap and coke, has about 3 percent. It's hard and brittle.
Wrought iron is the purest commercial iron, made by oxidising the impurities in a furnace lined with haematite.
Wrought iron: Fe₂O₃ + 3C → 2Fe + 3CO (impurities removed, limestone as flux)
Copper: from matte
Copper pyrites is roasted, then heated with silica in a reverberatory furnace. The iron goes off as FeSiO₃ slag.
What's left is copper matte: mainly Cu₂S with a little FeS.
Copper: self-reduction
In a silica-lined converter, hot air is blown through the matte.
Some Cu₂S becomes Cu₂O, which then reacts with the remaining Cu₂S to give copper. Copper reduces itself!
Escaping SO₂ leaves blisters on the solid metal, so it's called blister copper.
Trap: why not reduce Cu₂S with carbon?
Carbon can't reduce Cu₂S well: CS₂ is less stable than Cu₂S, so ΔG isn't favourable.
That's why copper is made by self-reduction, after partial roasting.
Zinc
Zinc blende is roasted to zinc oxide, then reduced with coke at 673 kelvin.
Zinc's boiling point is low, so it comes off as vapour. It's distilled off and collected by rapid chilling.