Explanation
Pick the method by the difference
Concentration removes gangue. The method depends on how the ore differs from the gangue.
Density, magnetism, how well it wets, or how it dissolves.
Hydraulic washing
This is gravity separation. An upward stream of running water washes the powdered ore.
The lighter gangue is carried away, and the heavier ore particles stay behind.
Magnetic separation
If either the ore or the gangue is magnetic, a magnetic roller pulls them apart on a conveyor belt.
It's used for iron ores like magnetite.
Froth flotation
This is for sulphide ores. The powdered ore is mixed with water, a collector and a froth stabiliser, then air is blown in.
The ore particles are wetted by oil and rise into the froth. The gangue is wetted by water and sinks.
Depressants
To separate two sulphides, add a depressant.
Sodium cyanide stops zinc sulphide from entering the froth, but lets lead sulphide through.
Leaching: bauxite (Bayer process)
Leaching dissolves the ore in a reagent that leaves the gangue behind.
Bauxite is digested with hot concentrated sodium hydroxide at 473 to 523 kelvin. Alumina dissolves as sodium aluminate.
Silica dissolves too, as sodium silicate, but stays in solution later on.
Getting alumina back
The aluminate solution is neutralised with carbon dioxide. Hydrated alumina precipitates, helped by adding a little fresh seed.
Heating it at 1470 kelvin gives pure alumina.
Leaching silver and gold
Silver and gold are leached with dilute sodium or potassium cyanide in the presence of air. They dissolve as cyanide complexes.
Then zinc is added. Zinc is more reactive, so it pushes the silver or gold out as metal.